Method for restoring portion of turbine component

作者: Thomas Joseph Kelly

DOI:

关键词: Component (thermodynamics)Substrate (building)Structural engineeringResidualTurbineAirfoilComposite materialMaterials scienceWall thickness

摘要: A method for restoring a removed portion (58) of the airfoil wall (12) turbine component (10). This comprises following steps: (a) providing (10) comprising an having metal substrate (30) with thickness (66), wherein has been so as to provide residual (72); (b) composition (80) that at least substantially matches and (c) applying (72) such (80): (1) is adhered thickness; (2) restores (58). Also provided previously repaired

参考文章(53)
Joseph H. Bowden, Lawrence J. Roedl, Method for repairing an air cooled turbine engine airfoil ,(1997)
Robert Glenn Adinolfi, Melvin Chester Barlow, Raymond Merriman Hammond, Chemical milling using an inert particulate and moving vessel ,(1985)
Seetharamaiah Mannava, Bangalore Aswatha Nagaraj, Bhupendra Kumar Gupta, Method for repairing a thermal barrier coating ,(1997)
Shinji Kawasaki, Makoto Murai, Yasufumi Aihara, Process for the production of lanthanum chromite films by plasma spraying ,(1992)
Jackie Lee King, Raymond William Heidorn, Thomas Edward Mantkowski, Nripenda Nath Das, High temperature vapor coating container ,(1998)
Henry Lada, Robert E. Fishter, Brian A. Manty, Chemical milling of high tungsten content superalloys ,(1980)
William Scott Walston, Ramgopal Darolia, Jeffrey Allan Pfaendtner, Compositions and single-crystal articles of hafnium-modified and/or zirconium-modified nickel-base superalloys ,(2000)