摘要: Abstract In order to improve mechanical properties and optimize composition of TiAl−Nb alloys, Ti46Al5Nb0.1B alloys with different contents Fe (0, 0.3, 0.5, 0.7, 0.9, 1.1 at.%) were prepared by melting. Macro/microstructure compression the systematically investigated. Results show that element can decrease grain size, aggravate Al-segregation also form Fe-rich B2 phase in interdendritic area. Compressive testing results indicate Ti46Al5Nb0.1B0.3Fe alloy shows highest ultimate compressive strength fracture strain, which are 1869.5 MPa 33.53%, respectively. The improved is ascribed refinement solid solution strengthening Fe, strain due reduced lattice tetragonality γ alloys. However, excessive addition decreases caused severe Al-segregation.