Process for preparation of copper-iron-aluminum hydrogenation catalyst

作者: Yukiko Nawashiro heir by , Fumiaki Miya heir by , Bunji Miya

DOI:

关键词: Salt (chemistry)CalcinationMetal ions in aqueous solutionDissolutionCatalysisChemistryAlkali metalAqueous solutionInorganic chemistryFerrous

摘要: A process for the preparation of copper-iron-aluminum hydrogenation catalysts comprises step of: dissolving a cupric salt, ferrous salt and an aluminum in water urea resulting aqueous solution such amount that mole number is at least 0.7 time as large sum equivalents metal ions, heating mixed solution, further continuing until pH liquid 4.6 to 7.5, adding alkali reaction elevate 9.5 11.5, conducting then separating, water-washing, drying calcining formed precipitate.

参考文章(1)
Yuzi Sawamoto, Shizuo Hisamitsu, Kunizo Hashiba, Bunji Miya, Process for preparation for copper-iron-aluminum catalysts and catalysts prepared by the process ,(1977)