作者: Jinbao Lin , Qudong Wang , Liming Peng , Hans J. Roven
DOI: 10.1016/J.JALLCOM.2008.09.031
关键词: Ultimate tensile strength 、 Ductility 、 Alloy 、 Strain rate 、 Microstructure 、 Extrusion 、 Fiber 、 Materials science 、 Metallurgy 、 Texture (crystalline)
摘要: Abstract The microstructure and texture development of an extruded ZK60 Mg alloy during cyclic extrusion compression (CEC) at 230 °C was investigated. Tensile tests were performed room temperature a strain rate 1 × 10−3 s−1. results show that the effectively refined by CEC processing. initial fiber became disintegrated processing developed new texture. After 4-passes, elongation-to-failure significantly increased almost three times compared with as-extruded alloy. Texture change grain refinement considered to be responsible for large tensile ductility in processed Furthermore, smaller intensity specimen may another reason ductility.