摘要: Elemental sulfur produced by chloride leaching of sulfide ores or concentrates contains selenium and tellurium usually too high to be used in various industrial agricultural uses. The the residue can upgraded 90% grade froth flotation concentration followed purification removal. is a form discrete particles with size range 5 10 microns. tend agglomerate pulp hence mechanically entrap gangue minerals. With sodium silicate as dispersant well depressant for siliceous material, concentrate recovery obtained single-stage flotation. reagent consumptions are minimum. majority chalcopyrite remains tailings readily recovered different reagents. When amyl xanthate used, 85% copper 14.5% sent back circuits.

参考文章(8)
AJ Parker, RL Paul, GP Power, Electrochemical aspects of leaching copper from chalcopyrite in ferric and cupric salt solutions Australian Journal of Chemistry. ,vol. 34, pp. 13- 34 ,(1981) , 10.1071/CH9810013
J.E. Dutrizac, R.J.C. MacDonald, Ferric ion as a leaching medium Miner. Sci. Eng., v. 6, no. 2, pp. 59-100. ,vol. 6, pp. 59- 95 ,(1974)
Norman L. Weiss, SME mineral processing handbook Society of Mining Engineers of the American Institute of Mining, Metallurgical, and Petroleum Engineers. ,(1985)
B. R. Palmer, C. O. Nebo, M. F. Rau, M. C. Fuerstenau, Rate phenomena involved in the dissolution of chalcopyrite in chloride bearing lixiviants Metallurgical and Materials Transactions B-process Metallurgy and Materials Processing Science. ,vol. 12, pp. 595- 601 ,(1981) , 10.1007/BF02654332
Niels C Christensen, Process of treating ores containing galena ,(1920)