作者: Pei Tang Zhao , Zhi Ming Du , Li Dong Wang , Wei Dong Fei
DOI: 10.4028/WWW.SCIENTIFIC.NET/AMR.299-300.692
关键词: Ultimate tensile strength 、 Composite material 、 Aluminium 、 Monocrystalline whisker 、 Whisker 、 Materials science 、 Coating 、 Deformation (engineering) 、 Extrusion 、 Composite number 、 General Engineering
摘要: The 6061Al matrix composites reinforced with SnO2-coated aluminum borate whisker were fabricated using squeeze casting method. The composites with different SnO2 coating contents were extruded successfully at 350°C with the extrusion rate of 18mm/s. The results show that the Sn particles at the interface as liquid state at extrusion temperature result in the reduction of the extrusion load and the decrease of the probability of whisker fracture during hot deformation process. Moreover, unlike many surface cracks can be seen in the extruded composite without whisker coating, the surface crack-free extruded rods can be obtained for composites with whisker coating. The ABOW/SnO/6061Al composites tensile properties increased obviously after extrusion.