PROCESS FOR THE PREPARATION OF AN ISOTROPIC POLYIMIDE FILM

作者: Masakazu Okahashi , Akimitsu Tsukuda , Charles M. Paulson Jr. , James R. Edman , Tsuneyoshi Miwa

DOI:

关键词: CastingIsotropyPolyimideStretch ratioCatalysisMaterials scienceTransverse directionPolyamic acidComposite materialOrganic solvent

摘要: Abstract not available for EP0628062Abstract of corresponding document: WO9317069An isotropic, biaxially stretched polyimide film prepared by casting a solution polyamic acid precursor in an organic solvent containing cyclization catalyst and dehydrating agent onto the surface support, imidizing to give continuous self-supporting gel 5-50 % weight solids, stretching machine direction (MD) at ratio 1.1-1.9, transverse (TD) with respect so as maintain TD/MD stretch from 0.9 1.3.

参考文章(4)
Ronald D. Goldblatt, Charles R. Davis, Jae M. Park, Polyamic acid structures, and methods of fabrication thereof ,(1991)
Tadao Muramatsu, Hiroshi Inoue, Yasuji Narahara, Tetsuji Hirano, Process for producing a shaped and drawn aromatic imide polymer article ,(1988)
Yoshihide Konookacho Ohnari, Koji Hieitsuji Okada, Junichi Hieitsuji Hazama, Toshinori Konookacho Mizuguchi, Polyimide resin film ,(1991)
Yoshihide Konookacho Ohnari, Koji Hieitsuji Okada, Junichi Hieitsuji Hazama, Toshinori Konookacho Mizuguchi, Resin film and method of making said film ,(1991)