Investigation of Combustion Kinetics of Five Waste Wood Samples with Thermogravimetric Analysis

作者: Sema Yurdakul Yorulmaz , Aysel Atimtay

DOI: 10.1007/978-3-540-95991-5_46

关键词: CombustibilityCombustion kineticsCharNuclear chemistryComposite materialThermogravimetric analysisWood wasteMaterials scienceCombustionActivation energyThermal decomposition

摘要: In the present study, combustion mechanisms, thermal kinetics, and phases of were investigated for untreated pine treated MDF, plywood particleboard samples. Waste wood samples combusted in air at 10, 20 30°C/min heating rates TGA. As a result TG analysis, decomposition was observed lower temperatures as compared to sample because catalyzing effects chemicals Therefore, there less flammable products, weight losses main oxidation region, decrease max. loss formation more char sample. other words, used during production these lead combustibility Thermal kinetic constants calculated by using Coats Redfern Broido Methods. order find out mechanisms responsible waste samples, six solid state Method tested.

参考文章(16)
R Zakrzewski, Pyrolysis kinetics of wood comparison of iso- and polythermal thermogravimetric methods Electronic Journal of Polish Agricultural Universities. Series Wood Technology. ,vol. 06, ,(2003)
Arno P. Schniewind, Concise encyclopedia of wood & wood-based materials Pergamon Press. ,(1989)
L.T Vlaev, I.G Markovska, L.A Lyubchev, Non-isothermal kinetics of pyrolysis of rice husk Thermochimica Acta. ,vol. 406, pp. 1- 7 ,(2003) , 10.1016/S0040-6031(03)00222-3
K.W. Ragland, D.J. Aerts, A.J. Baker, Properties of wood for combustion analysis. Bioresource Technology. ,vol. 37, pp. 161- 168 ,(1991) , 10.1016/0960-8524(91)90205-X
MING GAO∗, SHUYING LI, CAIYUN SUN, THERMAL DEGRADATION OF WOOD IN AIR AND NITROGEN TREATED WITH BASIC NITROGEN COMPOUNDS AND PHOSPHORIC ACID Combustion Science and Technology. ,vol. 176, pp. 2057- 2070 ,(2004) , 10.1080/00102200490514840
Joaquin Reina, Enrique Velo, Luis Puigjaner, Thermogravimetric study of the pyrolysis of waste wood Thermochimica Acta. ,vol. 320, pp. 161- 167 ,(1998) , 10.1016/S0040-6031(98)00427-4
J.T. Sun, Y.D. Huang, G.F. Gong, H.L. Cao, Thermal degradation kinetics of poly(methylphenylsiloxane) containing methacryloyl groups Polymer Degradation and Stability. ,vol. 91, pp. 339- 346 ,(2006) , 10.1016/J.POLYMDEGRADSTAB.2005.04.037
O.O. Sonibare, O.A. Ehinola ., R. Egashira ., Lim KeanGiap ., An Investigation into the Thermal Decomposition of Nigerian Coal Journal of Applied Sciences. ,vol. 5, pp. 104- 107 ,(2005) , 10.3923/JAS.2005.104.107
Manabendra Deka, C.N. Saikia, K.K. Baruah, Studies on thermal degradation and termite resistant properties of chemically modified wood. Bioresource Technology. ,vol. 84, pp. 151- 157 ,(2002) , 10.1016/S0960-8524(02)00016-0