Kaolin clay-based pigment

作者: Richard A. Slepetys , Fred R. Huege , David L. Catone

DOI:

关键词: AluminosilicateMixing (process engineering)BrightnessAnhydrousPigmentCoatingMineralogyAmorphous solidMaterials scienceChemical engineeringCalcination

摘要: A substantially white, anhydrous, amorphous aluminosilicate pigment is obtained by calcining a combination of previously uncalcined kaolin clay and an alumina source. The calcination carried out at temperature about 870° C. to 1400° C., preferably 1260° for suitable period time, e.g., 0.1 3 hours. pigments the foregoing method display enhanced brightness greater than merely additive which would be mixing with calcined are otherwise well suited use as paper-filling or coating pigments.

参考文章(8)
David G. Bell, Keith R. Gibson, Processing of kaolinitic clays at high solids ,(1978)
Tom A Cecil, Daniel A Jacobs, Method for bleaching gray kaolin clay ,(1969)
Robert H. Garner, Anthony D. McConnell, Anhydrous kaolin clay pigment and method of preparation ,(1981)
Jr. Robert B. Mixon, Kaolin clay processing ,(1979)
Hiroshi Umezaki, Hidekimi Kadokura, Pigmented aluminum oxide powder and method of producing the same ,(1983)
Robert W. Bradshaw, Brian R. Angel, Methods of producing kaolin pigments ,(1980)