作者: Hemant Borkar , Majid Hoseini , Mihriban Pekguleryuz
DOI: 10.1016/J.MSEA.2012.01.029
关键词:
摘要: Abstract Effect of Sr addition on hot deformation characteristics and texture evolution Mg–1 wt%Mn (M1) alloy is investigated with compression tests. additions up to 2 wt% M1 refine the as-cast microstructure. Flow curves M1–Sr alloys have been plotted at 400 °C 0.1/s strain rate which show softening behavior indicating dynamic recrystallization (DRX). The after strong basal in nature but it weakens increasing additions. This attributed particle-stimulated nucleation (PSN) recrystallization, induced by Mg–Sr intermetallics deformed