作者: Jing Zhang , Hao Huang , Wenxia Xiao , Chengbo Yang
DOI: 10.1080/02670836.2017.1363992
关键词:
摘要: ABSTRACTAn Mg–7.2Zn–1.5Cu–1.0Mn (wt-%) magnesium alloy was processed by extrusion and a subsequent solution heat treatment, followed two-step aging with the aim of achieving high ...