作者: M. Doner , H. Conrad
DOI: 10.1007/BF02644581
关键词:
摘要: The plastic flow of the commercial titanium material Ti-50A (0.5 at. pct Oeq) 22 μm grain size was investigated over temperature range 600 to 1150 structure) and strain rates 3 x 10-5 10-2 per s employing both constant rate cycling tests. Dynamic aging occurred in 850 (0.31 0.44Tm) with an activation energy 50 kcal mole derived from start serrations stress-strain curves, maxima hardening minima ductility. This value is accord that for diffusion oxygen titanium. At temperatures above (0.46 0.59Tm) data were very well represented by Weertman’s glide climb high creep mechanism, giving eskT/Dμb= 1.1 106 (σ/μ)4.55 withD = 1.0 exp (- 57,800/RT). 57.8 available self-diffusion