作者: DY Li , Rong Liu , None
DOI: 10.1016/S0043-1648(98)00388-3
关键词:
摘要: Abstract Recent studies show that pseudo-elastic TiNi alloy exhibits high resistance to wear, compared many conventional wear-resistant materials. It is demonstrated hardness not crucial the wear of this alloy, since its lower than those In order understand excellent behaviour and determine factors responsible for performance Ti–50.3 at.% Ni during a dry sliding process was investigated 2Cr13 steel. performed much better steel, although latter has higher hardness. expected attributable special mechanical behaviour, in particular so-called pseudo-elasticity, caused by reversible martensitic transformation. Mechanical thermal properties were studied FEM analysis made investigate plastic strain contact region correlate are influenced