Deactivation of Cu/ZnO/Al2O3 Catalyst: Evolution of Site Concentrations with Time

作者: CP Thurgood , JC Amphlett , RF Mann , BA Peppley

DOI: 10.1023/A:1023680121028

关键词:

摘要: The reforming of methanol is acknowledged as a convenient means to generate hydrogen for PEFC due the low temperature (<280 °C) at which reaction occurs and CO content reformate. However, catalyst prone deactivation in upper range its operating temperatures. This paper presents method analysis relative changes site concentrations are deduced from series long-duration rate measurements. sites involved shown evolve independently each other. In particular, concentration adsorption decline greater than those responsible oxygenated species. A key process decrease capacity adsorb dissociate hydrogen.

参考文章(6)
G.C. Chinchen, R.H. Logan, M.S. Spencer, Water-gas shift reaction over an iron oxide/chromium oxide catalyst. Applied Catalysis. ,vol. 12, pp. 89- 96 ,(1984) , 10.1016/S0166-9834(00)81506-7
Brant A. Peppley, John C. Amphlett, Lyn M. Kearns, Ronald F. Mann, Methanol–steam reforming on Cu/ZnO/Al2O3 catalysts. Part 2. A comprehensive kinetic model Applied Catalysis A-general. ,vol. 179, pp. 31- 49 ,(1999) , 10.1016/S0926-860X(98)00299-3
Brant A. Peppley, John C. Amphlett, Lyn M. Kearns, Ronald F. Mann, Methanol–steam reforming on Cu/ZnO/Al2O3. Part 1: the reaction network Applied Catalysis A-general. ,vol. 179, pp. 21- 29 ,(1999) , 10.1016/S0926-860X(98)00298-1
C.V. Ovesen, P. Stoltze, J.K. Nørskov, C.T. Campbell, A kinetic model of the water gas shift reaction Journal of Catalysis. ,vol. 134, pp. 445- 468 ,(1992) , 10.1016/0021-9517(92)90334-E
W. Curtis. Conner, John L. Falconer, Spillover in Heterogeneous Catalysis Chemical Reviews. ,vol. 95, pp. 759- 788 ,(1995) , 10.1021/CR00035A014