Influence of a CVD carbon coating on the mechanical property stability of Nicalon SiC fiber

作者: D.B. Fischbach , P.M. Lemoine

DOI: 10.1016/0266-3538(90)90092-J

关键词:

摘要: … From these observations it is concluded that: (i) the CVD carbon coating process causes … of the coating are favorable for a weak composite matrix interface, and (iii) the coating can also …

参考文章(15)
C.H. ANDERSSON, R. WARREN, THE STRENGTH AND ELASTIC MODULUS OF MULTIFILAMENT SiC FIBRES Advances in Composite Materials#R##N#Proceedings of the Third International Conference on Composite Materials, Held in Paris, 26–29 August 1980. pp. 1129- 1139 ,(1980) , 10.1016/B978-1-4832-8370-8.50090-5
L. C. Sawyer, R. Arons, F. Haimbach, M. Jaffe, K. D. Rappaport, Characterization of Nicalon®: Strength, Structure, and Fractography Ceramic engineering and science proceedings. ,vol. 6, pp. 567- 575 ,(2008) , 10.1002/9780470320280.CH9
Terence J. Clark, Michael Jaffe, James Rabe, Neal R. Langley, Thermal Stability Characterization of SiC Ceramic Fibers: I, Mechanical Property and Chemical Structure Effects 10th Annual Conference on Composites and Advanced Ceramic Materials: Ceramic Engineering and Science Proceedings, Volume 7, Issue 7/8. ,vol. 7, pp. 901- 913 ,(2008) , 10.1002/9780470320341.CH18
Linda C. Sawyer, Rong T. Chen, Frank Haimbach Iv, Paul J. Harget, Edward R. Prack, Michael Jaffe, Thermal Stability Characterization of SiC Ceramic Fibers: II, Fractography and Structure 10th Annual Conference on Composites and Advanced Ceramic Materials: Ceramic Engineering and Science Proceedings, Volume 7, Issue 7/8. ,vol. 7, pp. 914- 930 ,(2008) , 10.1002/9780470320341.CH19
Terence J. Clark, Richard M. Arons, James B. Stamatoff, James Rabe, Thermal Degradation of Nicalon™ SiC Fibers Proceedings of the 9th Annual Conference on Composites and Advanced Ceramic Materials: Ceramic Engineering and Science Proceedings, Volume 6, Issue 7/8. pp. 576- 588 ,(2008) , 10.1002/9780470320280.CH10
JONATHAN LIPOWTZ, H.A. FREEMAN, R.T. CHEN, E. R. PRACK, Composition and Structure of Ceramic Fibers Prepared from Polymer Precursors Advanced Ceramic Materials. ,vol. 2, pp. 121- 128 ,(1987) , 10.1111/J.1551-2916.1987.TB00066.X
R. CHAIM, A.H. HEUER, The Interface Between (Nicalon) SiC Fibers and a Glass‐Ceramic Matrix Advanced Ceramic Materials. ,vol. 2, pp. 154- 158 ,(1987) , 10.1111/J.1551-2916.1987.TB00072.X
Krishan L. Luthra, Thermochemical Analysis of the Stability of Continuous “SiC” Fibers Journal of the American Ceramic Society. ,vol. 69, ,(1986) , 10.1111/J.1151-2916.1986.TB07344.X
T. Mah, N. L. Hecht, D. E. McCullum, J. R. Hoenigman, H. M. Kim, A. P. Katz, H. A. Lipsitt, Thermal stability of SiC fibres (Nicalon Journal of Materials Science. ,vol. 19, pp. 1191- 1201 ,(1984) , 10.1007/BF01120029