Hydrogen effects in installed cables and under accelerated conditions

作者: A.D. Iddin , C.J. White , K.W. Plessner , S.J. Stannard-Powell

DOI: 10.1049/IP-J:19860019

关键词:

摘要: Attenuation increases have been measured on installed cables containing high-phosphorus doped fibres, mainly at wavelengths above 1300 nm, the operating wavelength. The hydrogen concentration was determined in some of these cables, making possible a correlation with fibre-in-hydrogen tests. An accelerated aging test carried out which two types cable, each three fibre, were held 90°C. Using data from field measurements and test, it confirmed that results can be extrapolated to low pressures present cables. upper limit for degradation single-mode fibre after long period cable calculated, shown negligible.

参考文章(1)
K.W. Plessner, S.J. Stannard-Powell, Attenuation/time relation for OH formation in optical fibres exposed to H2 Electronics Letters. ,vol. 20, pp. 250- 252 ,(1984) , 10.1049/EL:19840168