Mechanical properties of alumina fiber/glass matrix composites with and without a tin dioxide interface

作者: Ramanan Venkatesh

DOI: 10.1016/S0921-5093(99)00115-X

关键词:

摘要: Abstract Alumina+zirconia (PRD-166) and Saphikon fibers reinforced glass matrix composites with without a SnO 2 interphase were prepared by slurry infiltration their mechanical characteristics evaluated. Longitudinal bend strength increased volume fraction of in both PRD-166/glass PRD-166/SnO /glass composites. failed brittle manner whereas exhibited non-planar failure crack deflection fiber bridging as major toughening mechanisms. Saphikon/SnO tough extensive pullout. The difference the mode between was due to roughness. toughness deflection, bridging, partial debonding some Major mechanisms pullout minor contributions bridging.

参考文章(28)
R. W. Rice, Ceramic Matrix Composite Toughening Mechanisms: An Update Proceedings of the 9th Annual Conference on Composites and Advanced Ceramic Materials: Ceramic Engineering and Science Proceedings, Volume 6, Issue 7/8. ,vol. 6, pp. 589- 607 ,(2008) , 10.1002/9780470320280.CH11
Krishan K. Chawla, Ceramic Matrix Composites Springer, New York, NY. pp. 249- 292 ,(1993) , 10.1007/978-0-387-74365-3_7
Paul D. Jero, Ronald J. Kerans, Triplicane A. Parthasarathy, Effect of Interfacial Roughness on the Frictional Stress Measured Using Pushout Tests Journal of the American Ceramic Society. ,vol. 74, pp. 2793- 2801 ,(1991) , 10.1111/J.1151-2916.1991.TB06845.X
Hsin-Fu Wang, John C. Nelson, Chien-Li Lin, William W. Gerberich, INTERFACIAL STABILITY AND MECHANICAL PROPERTIES OF AL2O3 FIBER REINFORCED TI MATRIX COMPOSITES Journal of Materials Research. ,vol. 9, pp. 498- 503 ,(1994) , 10.1557/JMR.1994.0498
A Mechanism for the Control of Crack Propagation in All-Brittle Systems Proceedings of The Royal Society A: Mathematical, Physical and Engineering Sciences. ,vol. 282, pp. 508- 520 ,(1964) , 10.1098/RSPA.1964.0248
P.D. Jero, R.J. Kerans, The contribution of interfacial roughness to sliding friction of ceramic fibers in a glass matrix Scripta Metallurgica Et Materialia. ,vol. 24, pp. 2315- 2318 ,(1990) , 10.1016/0956-716X(90)90085-U
T.J. Mackin, P.D. Warren, A.G. Evans, Effects of fiber roughness on interface sliding in composites Acta Metallurgica Et Materialia. ,vol. 40, pp. 1251- 1257 ,(1992) , 10.1016/0956-7151(92)90424-D
James C. Romine, New High-Temperature Ceramic Fiber 11th Annual Conference on Composites and Advanced Ceramic Materials: Ceramic Engineering and Science Proceedings, Volume 8, Issue 7/8. ,vol. 8, pp. 755- 765 ,(2008) , 10.1002/9780470320402.CH31
Thomas J. Mackin, Jingyu Yang, Paul D. Warren, Influence of Fiber Roughness on the Sliding Behavior of Sapphire Fibers in TiAl and Glass Matrices Journal of the American Ceramic Society. ,vol. 75, pp. 3358- 3362 ,(1992) , 10.1111/J.1151-2916.1992.TB04434.X