作者: Hiroshi Sagane , Toshio Oguni
DOI:
关键词:
摘要: A resin composition comprises 1 to 60 parts by weight of a wollastonite fiber (in which the number-average length is 30 μm, diameter 0.1 10 and proportion number having 5 25 μm relative total 20 75%) an acid- or epoxy-modified olefinic melting point 100 170° C., thermoplastic (e.g., polycarbonate-series resin). The weight-average molecular modified may be about 2.5×10 4 30×10 . comprise flame retardant. combination use improves heat resistance, impact resistance weld strength, even in case using 7 average aspect ratio 1.5 3. present invention provides for improving strength surface property without deteriorating resistance.