作者: M.G. Barker , D.J. Wood
DOI: 10.1016/0022-5088(74)90243-4
关键词:
摘要: The corrosion products NaCrO/sub 2/ and Na/sub 4/FeO/sub 3/ were observed on the surfaces of chromium, iron, stainless steel after exposure to liquid sodium at 600 deg C above. identified by x-ray diffraction without removal covering layer. (8 figures) (auth)