Dry-jet wet spinning of fibers including two steps of stretching before complete coagulation

作者: Kigen Kawai

DOI:

关键词:

摘要: A method of making a fiber involves the sequential steps of: a) extruding as stream solution polymer having concentration 4-24 weight % into non-coagulating fluid; b) stretching while in fluid at spinning draft 25-2000; c) increasing by least 2 to 20-65 %; e) stretch ratio 1.5-10; and f) sufficiently form fiber.

参考文章(17)
Jong T. Park, Ink S. Han, Hak M. Kim, Moo S. Rhim, Seog C. Yoo, Ho J. Park, Du H. Kim, Sang H. Kim, Si M. Kim, Sa Ng B. Park, Two-stage process for preparing aromatic polyamide fiber ,(1987)
Leslie William Gulrich, Thomas Irvin Bair, Aramid spinning process ,(1984)
L. S. Li, L. F. Allard, W. C. Bigelow, On the morphology of aromatic polyamide fibers (Kevlar, Kevlar-49, and PRD-49) Journal of Macromolecular Science, Part B. ,vol. 22, pp. 269- 290 ,(1983) , 10.1080/00222348308215504
M. Panar, P. Avakian, R. C. Blume, K. H. Gardner, T. D. Gierke, H. H. Yang, Morphology of poly(p‐phenylene terephthalamide) fibers Journal of Polymer Science Part B. ,vol. 21, pp. 1955- 1969 ,(1983) , 10.1002/POL.1983.180211006