摘要: PURPOSE To evaluate the three-body wear resistance of five commercially available dual-cured resin-based composite luting agents compared both in a dry state and after water storage. MATERIALS AND METHODS Six specimens each material were prepared tested for ACTA machine 250,000 cycles loss was measured with profilometer. Material under three conditions: storage, 6-month 12-month RESULTS One-way two-way ANOVA Tukey's HSD test multiple comparisons revealed significant differences resistance. Water storage did not significantly affect four materials. The order was: Cosmedent Insure > Vivadent Dual-Cement Kerr Porcelite Dual Cure Jeneric/Pentron Optec Luting Cement Chameleon Mirage FLC (P < or = 0.0001). rank could be readily predicted when based solely on manufacturers' reported physical specification data.