AQUEOUS COMPOSITION FOR FIRE-PROTECTION COATING

作者: Park Bong Kuk

DOI:

关键词:

摘要: Provided are a fireproof coating composition whose durability is improved by enhancing storage stability and which excellent in water fastness, its preparation method. The comprises 5-70 wt% of glass, 10-95 polymer solution, 0.5-50 water-collecting particle, wherein the surface characteristic identical to that solution for 12 hours or more glass particle dispersed solution. Preferably an aqueous at least one kind silicate such as sodium silicate, potassium etc., content 0.5-80 wt%. has viscosity 10 cps more. selected from having size 1 nm mm property hydrophilicity, porosity, water-solubility swelling cement, silica, lime, poly(vinyl alcohol), starch, cellulose, activated carbon, chitosan, chitin, gelatin, collagen, borax, boric acid, carbonate, bicarbonate, phosphate, etc.