作者: Syarifah Aminah Ismail , Noorina Hidayu Jamil , Kamarudin Hussin , Mohd Arif Anuar Mohd Salleh
DOI: 10.4028/WWW.SCIENTIFIC.NET/AMM.754-755.567
关键词:
摘要: This project deals with the experimental results of leaching Sn from solder dross by means using different concentration hydrochloric acid (HCl). Solder was sieved to obtain a mean particle size 75 μm. The powder obtained leached HCl aqueous solution. To optimize parameter required for recovery dross, initially bench scale studies were carried out varying concentration, stirring time and temperature. indicate that 98.7% 0.1M HCl, 24 hours at60°C solution