Effect of Holding Time on the Corrosion Potential of SS304

作者: Hadi Purwanto , Hanisah Manshor

DOI: 10.4028/WWW.SCIENTIFIC.NET/AMR.576.382

关键词:

摘要: Stainless steels suffer from classical sensitization when encounter at certain temperature which results in precipitation of chromium carbide along grain boundary with simultaneous depletion near boundaries. This study focused on corrosion potential test different condition. The degree was measured based thickness boundary. With increasing holding time, the zone also increases due to diffusion into solid solution. Corrosion showed that heated sample 700°C for 60 minutes resulted highest current density and shifted its more active potential. tend increase precipitation.

参考文章(7)
Th. Heumann, F. W. Diekötter, Untersuchungen über das elektrochemische Verhalten des Chroms in schwefelsauren Lösungen im Hinblick auf die Passivität Berichte der Bunsengesellschaft für physikalische Chemie. ,vol. 67, pp. 671- 680 ,(1963) , 10.1002/BBPC.19630670711
C. S. TEDMON, D. A. VERMILYEA, D. E. BROECKER, Technical Note Effect of Cold Work on Intergranular Corrosion of Sensitized Stainless Steel Corrosion. ,vol. 27, pp. 104- 106 ,(1971) , 10.5006/0010-9312-27.3.104
C. L. Briant, A. M. Ritter, The effects of deformation induced martensite on the sensitization of austenitic stainless steels Metallurgical Transactions A. ,vol. 11, pp. 2009- 2017 ,(1980) , 10.1007/BF02655120
V.A. Safonov, E.V. Lapshina, T.H. Minh, S.Yu. Volosova, Specific Features of the Metal Passivation in Organic and Water-Organic Media Materials Science Forum. pp. 853- 860 ,(1995) , 10.4028/WWW.SCIENTIFIC.NET/MSF.185-188.853