High temperature behavior of functional TiAlBSiN nanocomposite coatings

作者: A.V. Pshyk , L.E. Coy , G. Nowaczyk , M. Kempiński , B. Peplińska

DOI: 10.1016/J.SURFCOAT.2016.07.075

关键词:

摘要: … Raman spectroscopy experiments were performed using … the crystalline phase led to growth of the amorphous phase. The thermodynamic driving force of the amorphous layer growth in …

参考文章(85)
N. Li, C. H. Gao, Formation and Crystallization Kinetics of Amorphous Alloys Springer, Berlin, Heidelberg. pp. 688- 694 ,(2009) , 10.1007/978-3-642-03653-8_223
Q Jane Wang, Yip-Wah Chung, None, Encyclopedia of tribology Springer. ,(2013)
Wei Yi Yang, Hiroaki Iwakuro, Hideichi Yagi, Tsukasa Kuroda, Shogo Nakamura, Study of Oxidation of TiSi2 Thin Film by XPS Japanese Journal of Applied Physics. ,vol. 23, pp. 1560- 1567 ,(1984) , 10.1143/JJAP.23.1560
J. Musil, Flexible hard nanocomposite coatings RSC Advances. ,vol. 5, pp. 60482- 60495 ,(2015) , 10.1039/C5RA09586G
J. P. Chu, C. T. Liu, T. Mahalingam, S. F. Wang, M. J. O’Keefe, B. Johnson, C. H. Kuo, Annealing-induced full amorphization in a multicomponent metallic film Physical Review B. ,vol. 69, pp. 113410- ,(2004) , 10.1103/PHYSREVB.69.113410
M. Pfeiler, J. Zechner, M. Penoy, C. Michotte, C. Mitterer, M. Kathrein, Improved oxidation resistance of TiAlN coatings by doping with Si or B Surface & Coatings Technology. ,vol. 203, pp. 3104- 3110 ,(2009) , 10.1016/J.SURFCOAT.2009.03.036
Carlo Paternoster, Alberto Fabrizi, Raimondo Cecchini, S. Spigarelli, Ph.V. Kiryukhantsev-Korneev, A. Sheveyko, Thermal evolution and mechanical properties of hard Ti–Cr–B–N and Ti–Al–Si–B–N coatings Surface & Coatings Technology. ,vol. 203, pp. 736- 740 ,(2008) , 10.1016/J.SURFCOAT.2008.08.013
Stan Veprek, Maritza J.G. Veprek-Heijman, Industrial applications of superhard nanocomposite coatings Surface & Coatings Technology. ,vol. 202, pp. 5063- 5073 ,(2008) , 10.1016/J.SURFCOAT.2008.05.038
Ph. V. Kiryukhantsev-Korneev, J. F. Pierson, J. Ph. Bauer, E. A. Levashov, D. V. Shtansky, Hard Cr-Al-Si-B-(N) coatings with oxidation resistance up to 1200°C Glass Physics and Chemistry. ,vol. 37, pp. 411- 417 ,(2011) , 10.1134/S1087659611040109
D. Philippon, V. Godinho, P.M. Nagy, M.P. Delplancke-Ogletree, A. Fernández, Endurance of TiAlSiN coatings: Effect of Si and bias on wear and adhesion Wear. ,vol. 270, pp. 541- 549 ,(2011) , 10.1016/J.WEAR.2011.01.009