Thermal oxidation of CP-Ti: Evaluation of characteristics and corrosion resistance as a function of treatment time

作者: Satendra Kumar , T.S.N. Sankara Narayanan , S. Ganesh Sundara Raman , S.K. Seshadri

DOI: 10.1016/J.MSEC.2009.03.007

关键词:

摘要: … to that of PN CP-Ti. The results of the present study further confirm the fact that thermally oxidized CP-Ti samples could offer excellent corrosion resistance compared to untreated CP-Ti. …

参考文章(33)
Per Kofstad, High temperature corrosion Elsevier. ,(1988)
H. Guleryuz, H. Cimenoglu, Surface modification of a Ti–6Al–4V alloy by thermal oxidation Surface & Coatings Technology. ,vol. 192, pp. 164- 170 ,(2005) , 10.1016/J.SURFCOAT.2004.05.018
G. P. Burns, Titanium dioxide dielectric films formed by rapid thermal oxidation Journal of Applied Physics. ,vol. 65, pp. 2095- 2097 ,(1989) , 10.1063/1.342856
L.M. Rabbe, J. Rieu, A. Lopez, P. Combrade, Fretting deterioration of orthopaedic implant materials: search for solutions Clinical Materials. ,vol. 15, pp. 221- 226 ,(1994) , 10.1016/0267-6605(94)90049-3
Stanley A. Brown, Paula J. Hughes, Katharine Merritt, In vitro studies of fretting corrosion of orthopaedic materials Journal of Orthopaedic Research. ,vol. 6, pp. 572- 579 ,(1988) , 10.1002/JOR.1100060415
D. Velten, V. Biehl, F. Aubertin, B. Valeske, W. Possart, J. Breme, Preparation of TiO2 layers on cp‐Ti and Ti6Al4V by thermal and anodic oxidation and by sol‐gel coating techniques and their characterization Journal of Biomedical Materials Research. ,vol. 59, pp. 18- 28 ,(2002) , 10.1002/JBM.1212
X Nie, E.I Meletis, J.C Jiang, A Leyland, A.L Yerokhin, A Matthews, Abrasive wear/corrosion properties and TEM analysis of Al2O3 coatings fabricated using plasma electrolysis Surface & Coatings Technology. ,vol. 149, pp. 245- 251 ,(2002) , 10.1016/S0257-8972(01)01453-0
Marc Long, H.J Rack, Titanium alloys in total joint replacement—a materials science perspective Biomaterials. ,vol. 19, pp. 1621- 1639 ,(1998) , 10.1016/S0142-9612(97)00146-4
H Dearnley, PA, Dahm, KL, Cimenoglu, The corrosion–wear behaviour of thermally oxidised CP-Ti and Ti–6Al–4V Wear. ,vol. 256, pp. 469- 479 ,(2004) , 10.1016/S0043-1648(03)00557-X