作者: Yong K. Lee , Kangsoo Lee , Taeho Jung
DOI: 10.1016/J.ELECOM.2008.08.048
关键词:
摘要: Abstract The effects of pulsating current and voltage sources with different magnitudes on an oxide film formed by microarc oxidation (MAO) AZ31B magnesium alloy in alkaline metal silicate solution were investigated. thickness increased increasing source but the uniformity surface became worse. unstable process represented fluctuating established across was discussed related to roughness melting down alloy. By comparing a produced more uniform than source.