A review of field performance of EVA-based encapsulants

作者: R.T. Tucker , R.S. Yorgensen

DOI: 10.1109/PVSC.2002.1190948

关键词:

摘要: As part of a past PVMaT contract (ZAG-3-11219-02-105661), several encapsulant formulations, developed for enhanced photothermal stability, were fielded at the STAR facility (Arizona) long-term testing and observation. In all, 36 modules (4 different module manufacturers) have been evaluated. At annual evaluation point, had exposed in field 4.5 years. Visual inspection I-V measurements made each module. Upon inspection, all formulations designed to eliminate discoloring mechanism appeared be clear. The relative short-circuit current (I/sub sc/) was measured For types, it found that dependence Isc with exposure time same particular type, regardless exclusive formulation.

参考文章(2)
W.H. Holley, S.C. Agro, J.P. Galica, L.A. Thoma, R.S. Yorgensen, M. Ezrin, P. Klemchuk, G. Lavigne, Investigation into the causes of browning in EVA encapsulated flat plate PV modules world conference on photovoltaic energy conversion. ,vol. 1, pp. 893- 896 ,(1994) , 10.1109/WCPEC.1994.520105
Peter Klemchuk, Myer Ezrin, Gary Lavigne, William Holley, James Galica, Susan Agro, Investigation of the degradation and stabilization of EVA-based encapsulant in field-aged solar energy modules Polymer Degradation and Stability. ,vol. 55, pp. 347- 365 ,(1997) , 10.1016/S0141-3910(96)00162-0