作者: S. AKTA , G. J. RICHARDSON , C. M. SELLARS
DOI: 10.2355/ISIJINTERNATIONAL.45.1666
关键词:
摘要: The recrystallization kinetics of 3% Si steel after hot rolling and plane strain compression at rates from 0.05 to 5s-1 over a temperature range 800 1100°C have been investigated. flow stress the ferritic Indicates that dynamic recovery rate is about two orders magnitude faster than in austenite. Recrystallization affected by deformation variables strongly influenced initial grain size. In coarse grained material, retardation resulted appearance plateau curves. Austenite present during affects both strength subsequent kinetics.