作者: G. Giaccio , R. Zerbino , J.M. Ponce , O.R. Batic
DOI: 10.1016/J.CEMCONRES.2008.02.009
关键词:
摘要: … 5 and 19 mm, distributed in 3 equal fractions in accordance with ASTM C 1293. The control … of strength after 28 days, whereas in concretes with great damage produced by ASR, there is …