作者: Takayuki Hattori , Yoshihisa Mizumoto , Tetsuo Mizoguchi
DOI:
关键词:
摘要: A conductive elastomer composition includes an ionic-conductive component, which contains anion-containing salt having a fluoro group (F—) and sulfonyl (—SO2—). The has volume charge not more than 108.5 (Ω·cm) when the is measured at voltage of 100V applied theretoin accordance with method specified in JIS K6911. compression set 30% temperature 70° C. for 24 hours compressibility ratio 25% “the permanent testing methods rubber, vulcanized or thermoplastic” K6262.