Low shrink tension film

作者: Blaine C. Childress

DOI:

关键词:

摘要: A film includes a core layer including linear random alpha-olefin/vinyl aromatic copolymer; and first second outer layers an olefinic polymer; the having Young's modulus between 50,000 200,000 psi, free shrink 40 80% at 240°F, tension of 50 400 or force 20 180 grams, 240°F. First intermediate ethylene copolymer melt index less than 2.0 can be optionally included. Alternatively, 2.0; properties as disclosed above.

参考文章(13)
Mitchell J. Rackovan, Oscar C. Mascarenhas, Gerald G. Popely, Melvin S. Freedman, Cling films and articles ,(1997)
Kazuyuki Takimoto, Kenichi Morizono, Keiji Okada, Olefin copolymer shrink film ,(1998)
Martindale Nelson, Low shrink force shrink film ,(1990)
Walter Berndt Mueller, Low shrink energy films ,(1988)
Maurice W. Blackwelder, Louis M. DiBello, Multilayer label material ,(1997)
Walter Berndt Mueller, Linear polyethylene shrink films ,(1983)
Eugene F. Lucas, David H. Anderson, Vincent E. Carman, Fuel-efficient energy storage automotive drive system ,(1980)