The behaviour of thiocyanate and cyanate during jarosite precipitation

作者: J.E. Dutrizac , D.J. Hardy

DOI: 10.1016/S0304-386X(96)00079-5

关键词:

摘要: Abstract The behaviour of thiocyanate and cyanate during the precipitation potassium jarosite was investigated. Thiocyanate strongly complexes dissolved ferric ion thereby reduces amount precipitated. composition jarosite, however, is virtually independent concentration,

参考文章(8)
Renato G. Bautista, Hydrometallurgical Process Fundamentals ,(1984)
A. J. Monhemius, J. E. Dutrizac, Iron Control In Hydrogenmetallurgy E. Horwood , Halsted Press. ,(1986)
C.A. Fleming, Hydrometallurgy of precious metals recovery Hydrometallurgy. ,vol. 30, pp. 127- 162 ,(1992) , 10.1016/0304-386X(92)90081-A
J.A. King, D.A. Knight, Autoclave operations at Porgera Hydrometallurgy. ,vol. 29, pp. 493- 511 ,(1992) , 10.1016/0304-386X(92)90029-Y
B.A. Wills, Precious and rare metal technologies Minerals Engineering. ,vol. 2, pp. 278- ,(1989) , 10.1016/0892-6875(89)90053-8
J. E. Dutrizac, Factors affecting alkali jarosite precipitation Metallurgical and Materials Transactions B-process Metallurgy and Materials Processing Science. ,vol. 14, pp. 531- 539 ,(1983) , 10.1007/BF02653939