作者: Y LENG , S CHAN , S JIANG , K KHOR
DOI: 10.1016/J.SSI.2004.02.026
关键词:
摘要: … With this method, expensive GDC powder is not required… SOFC with Ni-Gd 0.1 Ce 0.9 O 1.95 (GDC) as the anode and La 0.8 Sr 0.2 Co 0.2 Fe 0.8 O 3 (LSCF)-Gd 0.1 Ce 0.9 O 1.95 (GDC…