作者: Deividi Maurente Gomes da Silva , Vanessa Giaretton Cappellesso , Maurício Germano Lopes Garcia , Angela Borges Masuero , Denise Carpena Coitinho Dal Molin
DOI: 10.1590/S1678-86212021000200522
关键词:
摘要: Several factors, such as chemical shrinkage or environmental attack can produce concrete cracks. Calcium hydroxide content from the environment cement hydration promote self-healing phenomenon (SHP). This study evaluates calcium concentration influence on of cement-based materials. Cracked mortars with different types cement, a filler, pozzolanic, and high initial strength, were exposed to four conditions. Titration was method proposed determine amount leached in water, cracks closure analyzed by optical microscopy. CPII F (Portland Cement, type II, compound limestone) samples showed no trend Ca(OH) 2 leached, superficial cracking closure. Regarding CPV V, strength cement) samples, their behavior highest all exposure, submerged condition. Thus, significant cracks´ regarding presence Ca 2+ exposure environments, water source related this seems be primary factor improve SHP.