Hydrothermal treatment of polyamide 6 with presence of lanthanum chloride

作者: Zhi-liang Wang , Jia-li Xu , Qian Yuan , Mahmoud H. M. A. Shibraen , Jian Xu

DOI: 10.1007/S10118-016-1764-X

关键词:

摘要: Hydrothermal processing of polyamide 6 (PA6) with the presence lanthanum chloride (LaCl3) was studied in temperature region from 160 °C to 250 °C. PA6 will be dissolved superheated water when is above And as dissolved, hydrolysis happen, which makes chains degrade. By adding LaCl3 hydrothermal environment, intensify, especially higher than 200 When system cools down, hydrolyzed segments crystallize solution or remain depending on molecular weight. In addition, compound would affect crystallization proper size, and γ phase presented.

参考文章(23)
Marjoleine G.M. Wevers, Vincent B.F. Mathot, Thijs F.J. Pijpers, Bart Goderis, Gabriel Groeninckx, Full Dissolution and Crystallization of Polyamide 6 and Polyamide 4.6 in Water and Ethanol Progress in Understanding of Polymer Crystallization. ,vol. 714, pp. 151- 168 ,(2007) , 10.1007/3-540-47307-6_9
Zhi-liang Wang, Jia-li Xu, Lian-jia Wu, Xin Chen, Shu-guang Yang, Hui-chao Liu, Xian-ju Zhou, Dissolution, hydrolysis and crystallization behavior of polyamide 6 in superheated water Chinese Journal of Polymer Science. ,vol. 33, pp. 1334- 1343 ,(2015) , 10.1007/S10118-015-1682-3
Karine Charlet, Vincent Mathot, Jacques Devaux, Crystallization and dissolution behaviour of polyamide 6–water systems under pressure Polymer International. ,vol. 60, pp. 119- 125 ,(2011) , 10.1002/PI.2920
Marjoleine G.M. Wevers, Thijs F.J. Pijpers, Vincent B.F. Mathot, The way to measure quantitatively full dissolution and crystallization of polyamides in water up to 200 °C and above by DSC Thermochimica Acta. ,vol. 453, pp. 67- 71 ,(2007) , 10.1016/J.TCA.2006.10.020
Esther Vinken, Ann E. Terry, Otto van Asselen, Anne B. Spoelstra, Robert Graf, Sanjay Rastogi, Role of superheated water in the dissolution and perturbation of hydrogen bonding in the crystalline lattice of polyamide 4,6 Langmuir. ,vol. 24, pp. 6313- 6326 ,(2008) , 10.1021/LA800378C
H Bockhorn, A Hornung, U Hornung, P Jakobströer, M Kraus, Dehydrochlorination of plastic mixtures Journal of Analytical and Applied Pyrolysis. ,vol. 49, pp. 97- 106 ,(1999) , 10.1016/S0165-2370(98)00124-7
Yutaka Ikushima, Osamu Sato, Masahiro Sato, Kiyotaka Hatakeda, Masahiko Arai, Innovations in chemical reaction processes using supercritical water: an environmental application to the production of ε-caprolactam Chemical Engineering Science. ,vol. 58, pp. 935- 941 ,(2003) , 10.1016/S0009-2509(02)00631-0
Tianxi Liu, Hongdan Peng, Yue-E Miao, Weng Weei Tjiu, Lu Shen, Chun Wei, Synergistic effect of carbon nanotubes and layered double hydroxides on the mechanical reinforcement of nylon-6 nanocomposites Chinese Journal of Polymer Science. ,vol. 32, pp. 1276- 1285 ,(2014) , 10.1007/S10118-014-1521-Y