作者: Y.E. Gunanto , H. Sitompul , M.P Izaak , W.A. Adi
DOI: 10.1016/J.MATPR.2020.11.525
关键词:
摘要: Abstract We have succeeded to increase the absorption capacity of microwaves by substituting La3+ ions with Sr2+ (Ba0.6Sr0.4-xLaxFe10MnTiO19). Samples are made solid reaction method through milling. XRD is used characterize phase formation and crystal structure. SEM see surface morphology. VNA measure ability absorb microwaves. The results obtained indicate that sample single a hexagonal shape size particles still heterogeneous. −20.1 dB, −24.7 dB, −20.3 dB for × = 0.05, 0.10, 0.15 respectively.