Thermometric measurements of the self-field losses in silver sheathed PbBi2223 multifilamentary tapes

作者: A.E. Mahdi , T. Hughes , C. Beduz , Y. Yang , R.L. Stoll

DOI: 10.1109/77.620896

关键词:

摘要: Self-field ac losses in Ag sheathed PbBi-2223 tapes were measured using a thermometric method, which determines the by measuring temperature profile of vacuum insulated sample, with both ends at fixed temperature. In practice, samples placed capsule immersed LIN bath. By minimizing bath superheat, thermal emf and heating current contacts, loss induced increase as low 2 mK was Si diode thermometer. With typical sample length 600 mm, self-held between 7/spl times/10/sup -6/ W/m 4/spl -3/ different frequencies. The results are good agreement electric measurement theoretical calculation. This provides first independent confirmation that carefully voltage loops can give true sample.

参考文章(6)
P Dolez, M Aubin, D Willén, R Nadi, J Cave, Calorimetric ac loss measurements of silver sheathed Bi-2223 superconducting tapes Superconductor Science and Technology. ,vol. 9, pp. 374- 378 ,(1996) , 10.1088/0953-2048/9/5/007
Y. Yang, T. Hughes, C. Beduz, D.M. Spiller, R.G. Scurlock, W.T. Norris, The influence of geometry on self-field AC losses of Ag sheathed PbBi2223 tapes Physica C-superconductivity and Its Applications. ,vol. 256, pp. 378- 386 ,(1996) , 10.1016/0921-4534(95)00662-1
M. Ciszek, B.A. Glowacki, S.P. Ashworth, A.M. Campbell, J.E. Evetts, AC losses of Ag-(Bi,Pb)SrCaCuO-2223 tapes in combination of transverse external magnetic field and transport current IEEE Transactions on Applied Superconductivity. ,vol. 5, pp. 709- 712 ,(1995) , 10.1109/77.402646