作者: Norikane Yoshihiro , Saito Akira
DOI:
关键词:
摘要: A resin composition for solid freeform fabrication includes a thermoplastic resin, wherein the satisfies following conditions 1 and 2. 1. The has glass transition temperature (Tg) of 100 degrees C. or higher. molded object is dissolved in tetrahydrofuran at 25 within 24 hours mass ratio (the object/tetrahydrofuran) to 1/10 when heated 220 two hours.