Crack Initiation and Growth in HAZ of Microalloyed Steel

作者: K. Geric , S. Sedmak

DOI: 10.1007/1-4020-4972-2_522

关键词:

摘要: Due to welded joint microstructure heterogeneity it is very complex perform a its toughness test, because difficult position notch tip in the region of lowest toughness, and also control growing crack path.

参考文章(2)
L. P. Zhang, C. L. Davis, M. Strangwood, Effect of TiN particles and microstructure on fracture toughness in simulated heat-affected zones of a structural steel Metallurgical and Materials Transactions A-physical Metallurgy and Materials Science. ,vol. 30, pp. 2089- 2096 ,(1999) , 10.1007/S11661-999-0019-7
J. Neves, A. Loureiro, Fracture toughness of welds—effect of brittle zones and strength mismatch Journal of Materials Processing Technology. ,vol. 153, pp. 537- 543 ,(2004) , 10.1016/J.JMATPROTEC.2004.04.120