Magnetic properties and domain structures in domain refined grain‐oriented silicon steel (invited)

作者: T. Nozawa , Y. Matsuo , H. Kobayashi , K. Iwayama , N. Takahashi

DOI: 10.1063/1.340917

关键词:

摘要: The present paper is concerned with the development of low‐loss grain‐oriented silicon steel, and especially magnetic properties domain structures in refined steel. effects locally induced stress slight flux emergence have been examined as possible nucleation centers for effective walls which contribute to magnetization. fundamental phenomena their origins discussed on bases experimental facts. It was concluded that these refining were based upon interactions between subdomains having transverse magnetization, originate from free poles and/or internal stress, tensile steel orientation near (110)[001]. features both stack wound cores are described. Finally, a new technique raising degree (110)(001) introduced, approach minimum loss discussed.

参考文章(7)
H. J. Williams, R. M. Bozorth, W. Shockley, Magnetic Domain Patterns on Single Crystals of Silicon Iron Physical Review. ,vol. 75, pp. 155- 178 ,(1949) , 10.1103/PHYSREV.75.155
J. Shilling, W. Morris, M. Osborn, P. Rao, Orientation dependence of domain wall spacing and losses in 3-percent Si-Fe single crystals. IEEE Transactions on Magnetics. ,vol. 14, pp. 104- 111 ,(1978) , 10.1109/TMAG.1978.1059739
T. Nozawa, T. Yamamoto, Y. Matsuo, Y. Ohya, Relationship between total losses under tensile stress in 3 percent Si-Fe single crystals and their orientations near IEEE Transactions on Magnetics. ,vol. 14, pp. 252- 257 ,(1978) , 10.1109/TMAG.1978.1059767
T. Iuchi, S. Yamaguchi, T. Ichiyama, M. Nakamura, T. Ishimoto, K. Kuroki, Laser processing for reducing core loss of grain oriented silicon steel Journal of Applied Physics. ,vol. 53, pp. 2410- 2412 ,(1982) , 10.1063/1.330828
T. Nozawa, T. Yamamoto, Y. Matsuo, Y. Ohyo, Effects of scratching on losses in 3-percent Si-Fe single crystals with orientation near IEEE Transactions on Magnetics. ,vol. 15, pp. 972- 981 ,(1979) , 10.1109/TMAG.1979.1060287
T. Nozawa, T. Nakayama, Y. Ushigami, T. Yamamoto, Production of single-crystal 3% silicon-iron sheet with orientation near (110) [001] Journal of Magnetism and Magnetic Materials. ,vol. 58, pp. 67- 77 ,(1986) , 10.1016/0304-8853(86)90124-1