Atmospheric corrosion of magnesium (Mg) alloys

作者: M. Jönsson , D. Persson , Swerea Kimab

DOI: 10.1533/9780857091413.3.269

关键词:

摘要: Abstract: Depending on the atmospheric condition, and deposition of particles gases, this thin aqueous layer varies in thickness. In marine atmospheres other chloride containing environments, corrosion attacks are triggered by formation chloride-containing films surface. Gaseous constituents, such as CO2 more important conditions, compared to magnesium alloys bulk solutions. The microstructure is also vital importance behaviour conditions. However, conditions electrolyte thin, which decreases possibility galvanic coupling alloy constituents located at larger distances from each other.

参考文章(42)
Liu-Ying Wei, Development of microstructure in cast magnesium alloys Chalmers University of Technology. ,(1990)
Hugh P. Godard, The corrosion of light metals Wiley. ,(1967)
R. Winston Revie, Herbert Henry Uhlig, Uhlig's Corrosion Handbook ,(2005)
Martin Jönsson, Dan Persson, Rolf Gubner, The Initial Steps of Atmospheric Corrosion on Magnesium Alloy AZ91D Journal of The Electrochemical Society. ,vol. 154, ,(2007) , 10.1149/1.2779957
Wenjuan Liu, Fahe Cao, Bingli Jia, Liyun Zheng, Jianqing Zhang, Chunan Cao, Xiaogang Li, Corrosion behaviour of AM60 magnesium alloys containing Ce or La under thin electrolyte layers. Part 2: Corrosion product and characterization Corrosion Science. ,vol. 52, pp. 639- 650 ,(2010) , 10.1016/J.CORSCI.2009.10.030
Guangling Song, Andrej Atrens, Xianliang Wu, Bo Zhang, Corrosion behaviour of AZ21, AZ501 and AZ91 in sodium chloride Corrosion Science. ,vol. 40, pp. 1769- 1791 ,(1998) , 10.1016/S0010-938X(98)00078-X
S.J. Splinter, N.S. McIntyre, P.A.W. van der Heide, T. Do, Influence of low level iron impurities on the initial interaction of water vapour with polycrystalline magnesium surfaces Surface Science. ,vol. 317, pp. 194- 202 ,(1994) , 10.1016/0039-6028(94)90266-6