作者: Bart Weber , Liuquan Yang , Steve E. Franklin , Feng-Chun Hsia , Fiona M. Elam
DOI: 10.1016/J.CARBON.2021.04.068
关键词:
摘要: … Corrosion of the coating at 1.5 V (corrosion rate 0.5 nm h −1 ) resulted in no changes to the nanoscale topography; whereas corrosion at 2.5 V (corrosion rate 26.4 nm h −1 ) caused the …