Process for the production of aluminum hydroxide of improved whiteness

作者: Neil Brown

DOI:

关键词:

摘要: Aluminium hydroxide of high whiteness is produced by (i) heating aluminium obtained from the Bayer process to a temperature 300 700° C. (ii) dissolving soluble fraction thus activated product at 85 275° in aqueous sodium form aluminate liquor containing an undissolved residue very fine boehmite, (iii) filtering said obtain clear solution supersaturated with respect dissolved alumina, (iv) cooling 50 80° and seeding crystallized induce further crystallization, (v) separating, washing drying crystals.

参考文章(4)
Maria-Emilia Garcia Clavel, Maria-Jesus Martinez Lope, Maria-Teresa Casais Alvarez, Continuous procedure of obtention of compounds of aluminum from aluminum silicates and other aluminum ores ,(1984)
Hiroshi Tabuchi, Masahide Mohri, Shinji Fujiwara, Alpha-alumina and method for producing the same ,(1996)
Jozsef Matyasi, Sandor Nemeth, Gyorgy Kaptay, Bela Kokeny, Laszlo Zsembery, Process for preparing alumina being suitable for layer chromatography ,(1979)