作者: T. Granzow , Th. Woike , W. Rammensee , M. Wöhlecke , M. Imlau
关键词:
摘要: We present measurements of the temperature dependence pyroelectric effect in congruently melting strontium-barium-niobate doped with cerium and chromium range relaxor phase-transition. The influence doping concentration on transition is shown discussed respect to internal strain fields.