摘要: Abstract Hi‐Nicalon™‐S SiC fiber strengths and Weibull moduli were measured after oxidation for up to 100 hours between 700° C and 1400° C in wet and dry air. SiO2 scale …

参考文章(117)
S. M. Dong, G. Chollon, C. Labrugère, M. Lahaye, A. Guette, J. L. Bruneel, M. Couzi, R. Naslain, D. L. Jiang, Characterization of nearly stoichiometric SiC ceramic fibres Journal of Materials Science. ,vol. 36, pp. 2371- 2381 ,(2001) , 10.1023/A:1017988827616
G CHOLLON, M CZERNIAK, R PAILLER, X BOURRAT, R NASLAIN, J. P PILLOT, R CANNET, A model SiC-based fibre with a low oxygen content prepared from a polycarbosilane precursor Journal of Materials Science. ,vol. 32, pp. 893- 911 ,(1997) , 10.1023/A:1018597432067
G. S. Corman, K. L. Luthra, Silicon Melt Infiltrated Ceramic Composites (HiPerComp Springer, Boston, MA. pp. 99- 115 ,(2005) , 10.1007/0-387-23986-3_5
G. A. Budnitskii, N. N. Machalaba, Some Research Trends at the Institute Fibre Chemistry. ,vol. 33, pp. 85- 95 ,(2001) , 10.1023/A:1019252617696
G CHOLLON, R PAILLER, R NASLAIN, F LAANANI, M MONTHIOUX, P OLRY, Thermal stability of a PCS-derived SiC fibre with a low oxygen content (Hi-Nicalon) Journal of Materials Science. ,vol. 32, pp. 327- 347 ,(1997) , 10.1023/A:1018541030308
Cédric Sauder, Ceramic Matrix Composites: Nuclear Applications Ceramic Matrix Composites. pp. 609- 646 ,(2014) , 10.1002/9781118832998.CH22
R. S. Hay, G. E. Fair, A. Hart, S. Potticary, R. Bouffioux, Kinetics of Passive Oxidation of Hi-Nicalon-S SiC Fibers in Wet Air: Relationships between SiO2Scale Thickness, Crystallization, and Fiber Strength Mechanical Properties and Performance of Engineering Ceramics and Composites VII. pp. 253- 260 ,(2012) , 10.1002/9781118217467.CH24
Tomohiro Tanaka, Shigeki Shibayama, Michio Takeda, Akira Yokoyama, Recent Progress of Hi‐Nicalon Type S Development John Wiley & Sons, Ltd. pp. 217- 223 ,(2008) , 10.1002/9780470294826.CH32
T. J. Delph, Intrinsic strain in SiO2 thin films Journal of Applied Physics. ,vol. 83, pp. 786- 792 ,(1998) , 10.1063/1.366759
Y. Gogotsi, M. Yoshimura, Oxidation and properties degradation of SiC fibres below 850 °C Journal of Materials Science Letters. ,vol. 13, pp. 680- 683 ,(1994) , 10.1007/BF00271233