作者: Sahira Vasquez , Mukhtar Ahmad , Mattia Petrelli , Martina Costa Angeli , Raheel Riaz
DOI:
关键词:
摘要: In this work, Schottky diodes based on amorphous indium-gallium-zinc-oxide (IGZO) were fabricated on cellulose microfiber paper substrate. Silver lines used as the Schottky barrier were printed, in parallel to thermally evaporated Cr/Au ohmic contact, using a dispense printer. The morphological and electrical characteristics of the devices are presented. The fabricated diodes exhibited rectification ratios ranging from 3.4 to 34.9 at ±1V with ON voltages that range from 1.1V to 1.4 V, for device lengths (Ag to Au distance) from 145 µm to 894 µm. The diodes were characterized in a temperature range between 25°C and 80°C. They showed a decrease of the ON current when increasing temperature, which is mainly attributed to the change of the cellulose microstructure. Indeed, an opposite of the ON current behavior was registered when the diode was realized on a polyimide substrate. The realized flexible paper …