Factors affecting the oxidation mode of stainless steels

作者: C. Lille , R. F. A. Jargelius-Pettersson

DOI: 10.1179/MHT.2000.17.2.016

关键词: MetallurgyMicrostructureOxideOptical microscopeSpectroscopyDew pointGlow-discharge optical emission spectroscopyAirflowMaterials scienceScanning electron microscope

摘要: Studies have been made to investigate what effect different factors on oxide formation stainless steels at 600–1,000°C in air. The include the of microstructure, airflow rate, surface preparations, residual oxides and variations dew point Scanning electron microscope (SEM) equipped with energy dispersive X-ray spectroscopy (EDS), glow discharge optical emission (GDOES) light (LOM) were used characterise oxides.

参考文章(8)
Royden Hales, The high temperature oxidation behaviour of austenitic stainless steels Materials and Corrosion-werkstoffe Und Korrosion. ,vol. 29, pp. 393- 399 ,(1978) , 10.1002/MACO.19780290603
G. C. Wood, F. H. Stott, Oxidation of alloys Materials Science and Technology. ,vol. 3, pp. 519- 530 ,(1987) , 10.1080/02670836.1987.11782263
Hidetaka Konno, Isao Saeki, Ryusaburou Furuichi, Breakaway of Type 430 Stainless Steel in Water Vapor/Oxygen Atmospheres at Elevated Temperatures Corrosion engineering. ,vol. 37, pp. 338- 345 ,(1988) , 10.3323/JCORR1974.37.6_338
Per Kofstad, High temperature corrosion Elsevier. ,(1988)
F. H. Stott, F. I. Wei, High temperature oxidation of commercial austenitic stainless steels Materials Science and Technology. ,vol. 5, pp. 1140- 1147 ,(1989) , 10.1179/MST.1989.5.11.1140
J. Litz, A. Rahmel, M. Schorr, Selective Carbide Oxidation and Internal Nitridation of the Ni-Base Superalloys IN 738 LC and IN 939 in Air Oxidation of Metals. ,vol. 30, pp. 95- 105 ,(1988) , 10.1007/BF00656646
A. L. Marasco, D. J. Young, The oxidation of iron-chromium-manganese alloys at 900C Oxidation of Metals. ,vol. 36, pp. 157- 174 ,(1991) , 10.1007/BF00938460