作者: ANIL V. VIRKAR , L. VISWANATHAN
DOI: 10.1111/J.1151-2916.1979.TB19123.X
关键词: Melting point 、 Penetration (firestop) 、 Chemical reaction 、 Materials science 、 Inorganic chemistry 、 Electrolyte 、 Ion 、 Membrane 、 Alkali metal 、 Sodium
摘要: The degradation of sodium ion conductors is more severe below the melting point and use ..beta..''-alumina, where neutralization reaction accomplished, should be avoided point. A specimen Na/sub 3/Zr/sub 2/Si/sub 2/ PO/sub 12/ was tested. Rapid penetration occurred but not above. Results indicate that rapid used as solid electrolyte membranes in sodium-sulfur batteries. (FS)