Sintering of silicon nitride using Mg and Be additives

作者: Robert A. Giddings , Charles D. Greskovich , Svante Prochazka , Richard J. Charles

DOI:

关键词: NitrogenBerylliumDispersion (chemistry)Green bodyMagnesiumMetallurgySilicon nitrideSinteringParticulatesMaterials science

摘要: Abstract of the Disclosure A particulate dispersion silicon nitride, magnesium additive and beryllium is formed into a green body sintered at temperature ranging from about 1800°C to 2200°C in sintering atmosphere nitrogen superatmospheric pressure producing with density 80% 100%.